An attempt has been made to evaluate the suitability of austempered ductile iron ADI as media material for grinding iron ore in a ball mill Spheroidal graphite SG iron balls are austenitised at 900 C for 60 minutes and given stepped austempering treatment at 280 C for 30 minutes and 60 minutes followed by 380 C for 60 minutes in each case